Solders Used by Area of Industry Served

SOLDER

Melting Range
(°C)

Industry Served

Company

SnAg

221 - 226

Automotive

Visteon (Ford)

SnAgBi

 

206 - 213

Military/Aerospace

Panasonic

Consumer

Hitachi

SnAgBiCu

 

Military/Aerospace

Panasonic (FA Controller?)

SnAgBiCuGe

 

Consumer

Sony

SnAgBiX

206 - 213

Consumer

Panasonic

SnAgCu

217

Automotive

Panasonic

 

Telecommunications

Nokia

Nortel

Panasonic

Toshiba

SnBi

138

Consumer

Panasonic

SnCu

227

Consumer

Panasonic

Telecommunications

Nortel

SnZn

198.5

Consumer

NEC

Panasonic

Toshiba